(02) 8021 3517 Send your job →
● Products and testing

How to mix ACTFLEX 989 CWP. Lump free is half the job.

1 min readFORSPEC Technical Team

The short version

  • Mix ACTFLEX 989 CWP with a drill, never by hand.
  • Once it is smooth, let it stand for 3 to 4 minutes, then mix for 1 more minute.
  • Pot life is about 2 hours.

A two-part cementitious membrane is a chemical mix, not a paint. The powder needs time to wet out fully. Roll it on too soon and you get pinholes and a thin film.

ACTFLEX 989 CWP Part A liquid and Part B powder being mixed with a drill and paddle
Mixing ACTFLEX 989 CWP

The steps

  1. Weigh it: 1 part of Part A liquid to 1.2 parts of Part B powder, by weight.
  2. Mix by machine until smooth and lump free.
  3. Let it stand for 3 to 4 minutes.
  4. Mix again for 1 minute, then start rolling.
Pot life
About 2 hours at 25°C
Recoat
4 to 6 hours
Tile
From 6 to 8 hours after the final coat
FORSPEC on Instagram · 29 Oct 2026Lump free is only half the mixLoads when you tap

Where this comes from

Email thisNewsletter

Systems, products and drawings

● Your job next

Got a job this applies to?

Send the drawings or a few photos. FORSPEC comes back with the system, the details and the products for your job, within 6 business hours.

On site with FORSPEC

@forspec.pc on Instagram →

More news

All news →
● The FORSPEC Brief · monthly

The month in waterproofing. In one email.

Code and standards changes, new products, new test reports and jobs from site. Once a month. No sales emails.

One email a month. Unsubscribe in one click. We never share your address.

Send us your job →☎